The plant adopts a preferential flotation process for lead and zinc separation.
After three-stage crushing, the ore enters a ball mill and hydrocyclone grinding circuit. Overflow slurry proceeds to flotation.
Lead minerals are floated first, followed by zinc flotation from the tailings stream.
Final concentrates are thickened and filtered for transportation.